  • 1.Reciprocating friction and wear behavior of Ti3AlC2 and Ti3AlC2/Al2O3 composites against AISI52100 bearing steel
    L. Wu, J.X. Chen, M.Y. Liu, Y.W. Bao, Y.C. Zhou, Wear 266 (2009) 158–166
  • 2.Thermal properties of single-phase Y2SiO5
    Ziqi Sun, Meishuan Li, Yanchun Zhou, J. Europ. Ceram. Soc., 29 (2009) 551–557
  • 3.Fracture toughness determination of Ti3Si(Al)C2 and Al2O3 using a single gradient notched beam (SGNB) method
    D.T. Wan, Y.W. Bao, J.Z. Peng, Y.C. Zhou, J. Europ. Ceram. Soc., 29 (2009) 763–771
  • 4.Hydrolysis and Dispersion Properties of Aqueous Y2Si2O7 Suspensions
    Z.Q. Sun, X.W. Zhu, M.S. Li, Y.C. Zhou and Yoshio Sakka, J. Am. Ceram. Soc., 92 [1] 54–61 (2009)
  • 5.Tribological Properties of a Zr2Al3C4 Ceramic at Ambient Temperature
    L. Wu, L.F. He, Y.W. Bao and Y.C. Zhou, J. Am. Ceram. Soc.,92 [1] 141–146 (2009)
  • 6.Low-temperature instability of Ti2SnC: A combined transmission electron microscopy, differential scanning calorimetry, and x-ray diffraction investigations
    J. Zhang, B. Liu, J. Y. Wang, Y .C. Zhou, J. Mater. Res.,24 [1] 39-49 (2009)
  • 7.Mechanical and Thermophysical Properties of Zr–Al–Si–C Ceramics
    L.F. He, Y.W. Bao, J.Y Wang, M.S. Li, Y.C. Zhou, J. Am. Ceram. Soc.,92 [2] 445–451 (2009)
  • 8.Crystal Structure and Electronic Structure of a Novel Hf3AlN Ceramic
    F. Z. Li, C. F. Hu, J. M. Wang, B. Liu, J. Y. Wang, Y. C. Zhou, J. Am. Ceram. Soc., 92 [2] 476–480 (2009)
  • 9.Chemical bonding and mechanical properties of M2AC (M = Ti, V, Cr, A = Al, Si, P, S) ceramics from first-principles investigations
    T. Liao,J.Y. Wang and Y.C. Zhou, J. Mater. Res., 24 [2] 556-564 (2009)
  • 10.Current Status in Layered Ternary Carbide Ti3SiC2, (a Review)
    H.B. Zhang, Y.W. Bao and Y.C. Zhou, J. Mater. Sci. Technol., 25 [1] 1-38 (2009)
  • 11.Tribological properties of γ-Y2Si2O7 ceramic against AISI 52100 steel and Si3N4 ceramic counterparts
    Z. Q. Sun, L. Wu, M. S. Li, Y. C. Zhou, Wear, 266:960-967 (2009)
  • 12.Highly conductive and strengthened copper matrix composite reinforced by Zr2Al3C4 particulates
    J. Zhang, L. F. He, Y. C. Zhou, Scripta Mater., 20:976-979 (2009)
  • 13.Direct diffusion bonding of Ti3SiC2 and Ti3AlC2
    X. H. Yin, M. S. Li, J. J. Xu, J. Zhang, Y. C. Zhou, Mater. Res. Bull, 44:1379-1384 (2009)
  • 14.Amorphization by dislocation accumulation in shear bands
    Z.J. Lin, M.J. Zhuo, Z.Q. Sun, P. Veyssie`re, Y. C. Zhou, Acter. Mater, 57:2851-2857 (2009)
  • 15.Microstructure and mechanical and thermal properties of ternary carbides in Hf–Al–C system
    L.F. He, Y.W. Bao, J.Y. Wang, M. S. Li, Y. C. Zhou, Acter. Mater, 57:2765-2774 (2009)
  • 16.High-temperature internal friction, stiffness and strength of Zr–Al(Si)–C ceramics
    L.F. He, X.P. Lu, Y.W. Bao, J.Y. Wang and Y.C. Zhou, Scripta Mater., 61 (2009) 60–63
  • 17.Molten Salt Synthesis of Magnesium Aluminate (MgAl2O4) Spinel on Ti3AlC2 Substrate
    J. Zhang, D.H. Li, and Y.C. Zhou, J. Am. Ceram. Soc., 92 [5] 1074–1078 (2009)
  • 18.Recent Progress in Theoretical Prediction, Preparation, and Characterization of Layered Ternary Transition-Metal Carbides
    J.Y. Wang and Y.C. Zhou, Annu. Rev. Mater. Res., 39 (2009) 10.1-10.29(a Review)
  • 19.Theoretical investigation of A-element atom diffusion in Ti2AC (A=Sn, Ga, Cd, In, and Pb)
    B. Liu, J. Y. Wang, J. Zhang, J. M. Wang, F. Z. Li, Y. C. Zhou, Appl. Phys. Lett., 94(2009) 181906
  • 20.Effect of Al dopant on the hydrothermal oxidation behavior of Ti3SiC2 powders
    H.B. Zhang, X. Wang, C. Berthold, K.G. Nickel, Y.C. Zhou, J. Europ. Ceram. Soc.,29 (2009) 2097–2103
  • 21.Joining of Ti–Al–C ceramics by oxidation at low oxygen partial pressure
    A.J. Li, C.F. Hu, M.S. Li, Y.C. Zhou, J. Europ. Ceram. Soc.,29 (2009) 2619–2625
  • 22.Atomic-scale studies of native point defect and nonstoichiometryi n silicon oxynitride
    B. Liu, J.Y.Wang, F.Z.Li, Q.F.Tong, Y.C.Zhou, J. Phys. & Chem. Solid.,70(2009)982–988
  • 23.Surface Chemistry, Dispersion Behavior, and Slip Casting of Ti3AlC2 Suspensions
    Z. Q. Sun, M. S. Li, L. F. Hu, X. P. Lu, Y. C. Zhou, J. Am. Ceram. Soc., 92 [8] 1695–1702 (2009)
  • 24. A polysilazane coating protecting polyimide from atomic oxygen and vacuum ultraviolet radiation erosion
    L. F. Hu, M. S. Li, C. H. Xu, Y. M. Luo, Y. C. Zhou, Surface & Coatings Technology 203 (2009) 3338–3343
  • 25. Effects of Vacuum Ultraviolet Radiation on Atomic Oxygen Erosion of Polysiloxane/SiO2 Hybrid Coatings
    L. F. Hu, M. S. Li, Y. C. Zhou, J. Mater. Sci. Technol., 25[4] 483–488 (2009)
  • 26. Effect of Ti5Si3 on wear properties of Ti3Si(Al)C2
    Y. L. Liu, J. X. Chen, Y. C. Zhou, J. Europ. Ceram. Soc., 29 (2009) 3379–3385
  • 27. Effect of interstitial lithium atom on crystal and electronic structure of silicon oxynitride
    B. Liu, J. Y. Wang,F. Z. Li, H. Q. Nian, Y. C. Zhou, J Mater Sci., (2009) 44:6416–6422
  • 28.Reactive Hot Pressing and Properties of Nb2AlC
    W. Zhang, Nahum Travitzky, C. F. Hu, Y. C. Zhou, and Peter Greilz, J. Am. Ceram. Soc., 92 [10] 2396–2399 (2009)
  • 29. First-principles study of oxygen incorporation and migration mechanisms in Ti2AlC
    T,Liao, J. Y. Wang, M. S. Li, Y. C. Zhou, J. Mater. Res., 24 [10] 3190–3196 (2009)
  • 30. Mechanical and Thermal Properties of Antiperovskite Ti3AlC Prepared by an In Situ Reaction/Hot-Pressing Route
    X. W. Zhang, X. H. Wang, F. Z. Li, Y. C. Zhou, J. Am. Ceram. Soc., 92 [11] 2698–2703 (2009)
  • 31.Zirconium Aluminum Carbides: New Precursors for Synthesizing ZrO2–Al2O3 Composites
    L.F. He, Y.W. Bao, Y.C. Zhou, J. Am. Ceram. Soc., 92 [11] 2751–2758 (2009)
  • 32. High-temperature powder x-ray diffraction experiments and ab initio calculation of Ti3AlC2
    H. B. Zhang, X. Wu, Klaus Georg Nickel, J. X. Chen, Volker Presser1, J. Appl. Phys., 106(2009):013519