发 表 论 文
  申 请 专 利
  研 究 亮 点

2004 2005 2006 2007 2008 2009
2010 2011        
           
  • 1.Hot corrosion of γ-Y2Si2O7 in strongly basic Na2CO3 molten salt environment
    Z. Q. Sun, M.S. Li, Z.P. Li, Y.C. Zhou, J. Europ. Ceram. Soc., 28 (2008) 259–265
  • 2.Influence of water vapor on the oxidation behavior of Ti3AlC2 and Ti2AlC
    Z.J. Lin, M.S. Li, J.Y. Wang, Y.C. Zhou Scripta Materialia 58 (2008) 29–32
  • 3.A first-principles investigation of the phase stability of Ti2AlC with Al vacancies
    J.Y. Wang, Y.C. Zhou, T. Liao, J. Zhang, Z.J. Lin, Scripta Materialia 58 (2008) 227–230
  • 4.Effect of grain size, notch width, and testing temperature on the fracture toughness of Ti3Si(Al)C2 and Ti3AlC2 using the chevron-notched beam (CNB) method
    D.T. Wan, F.L. Meng, Y.C. Zhou, Y.W. Bao, J.X. Chen J. Europ. Ceram. Soc., 28 (2008) 663–669
  • 5.Evaluation of the elastic modulus and strength of unsymmetrical Al2O3
    Detian Wan, Yanchun Zhou, Yiwang Bao Mater. Sci. & Engin. A 474 (2008) 64–70
  • 6.High temperature corrosion behavior of a multilayer CrAlN coating prepared by magnetron sputtering method on a K38G alloy
    T.P. Li, Y.C. Zhou, M.S. Li, Z.P. Li Surface & Coatings Technology 202 (2008) 1985–1993
  • 7.In-situ reaction synthesis and decomposition of Ta2AlC
    C F Hu, J Zhang, Y W Bao, J Y Wang, M S Li and Y C Zhou Inter. J Mater. Res., 99 (2008) 8-13
  • 8.Titanium Silicon Carbide Pest Induced by Nitridation
    H B Zhang, Y C Zhou, Y W Bao and M S Li J. Am. Ceram. Soc., 91 [2] 494–499 (2008)
  • 9.Crystal Structure of V4AlC3: A New Layered Ternary Carbide
    C F Hu, J Zhang, J M Wang, F Z Li, J Y Wang and Y C Zhou, J. Am. Ceram. Soc., 91 [2] 636–639 (2008)
  • 10.Isothermal oxidation of bulk Zr2Al3C4 at 500 to 1000 °C in air
    L.F. He, Z.J. Lin, Y.W. Bao, M.S. Li, J.Y. Wang, and Y.C. Zhou J. Mater. Res., 23(2):359-366(2008)
  • 11.Preparation and properties of Si2N2O/ β -cristobalite composites
    Q F Tong, J Y Wang, Z P Li, Y C Zhou, J. Europ. Ceram. Soc., 28 (2008) 1227–1234
  • 12.Material removal and surface damage in EDM of Ti3SiC2 ceramic
    C.F. Hu, Y.C. Zhou, Y.W. Bao Ceramics International 34 (2008) 537–541
  • 13.Crystal structure and theoretical elastic property of two new ternary ceramics Hf3Al4C6 and Hf2Al4C5
    L.F. He, Z.J. Lin, J.Y. Wang, Y.W. Bao and Y.C. Zhou Scripta Materialia 58 (2008) 679–682
  • 14.Effect of LiYO2 on the synthesis and pressureless sintering of Y2SiO5
    Ziqi Sun, Yanchun Zhou and Meishuan Li J. Mater. Res., 23(3):732-736(2008)
  • 15.Phase stability, electronic structure and mechanical properties of ternary-layered carbide Nb4AlC3: An ab initio study
    J.M. Wang, J.Y. Wang, Y.C. Zhou, C.F. Hu Acta Materialia 56 (2008) 1511–1518
  • 16.Theoretical elastic stiffness of quaternary crystal Y3Si5N9O by first-principles investigation
    Jingyang Wang, Yanchun Zhou, Zhijun Lin, Takahisa Ohno, Phys. Rev. B 77, 104117 (2008)
  • 17.Microstructure and properties of bulk Ta2AlC ceramic synthesized by an in situ reaction/hot pressing method
    C. F. Hu, L. F. He, J Zhang, Y. W. Bao, J. Y. Wang, M. S. Li, Y. C. Zhou J. Europ. Ceram. Soc., 28 (2008) 1679–1685
  • 18.New MAX-Phase Compounds in the V–Cr–Al–C System
    Yanchun Zhou, Fanling Meng, Jie Zhang, J. Am. Ceram. Soc., 91 [4] 1357–1360 (2008)
  • 19.Microstructure, mechanical, and electrical properties of Cu–Ti3AlC2 and in situ Cu–TiCx composites
    Jie Zhang, Yanchun Zhou J. Mater. Res., 23(4)924-932 (2008)
  • 20.Stable M2AlC(0001) surfaces (M = Ti, V and Cr) by first-principles investigation
    J.M.Wang, J.Y. Wang, Y.C. Zhou J. Phys.: Condens. Matter 20 (2008) 225006 (11pp)
  • 21.Ab initio study of polymorphism in layered ternary carbide M4AlC3 (M = V, Nb and Ta)
    J.Y. Wang, J.M. Wang, Y.C. Zhou, Z.J. Lin, C.F. Hu Scripta Materialia 58 (2008) 1043–1046
  • 22.Surface strengthening of Ti3SiC2 through magnetron sputtering Cu and subsequent annealing
    H.P. Guo, J. Zhang, F.Z. Li, Y. Liu, J.J. Yin, Y.C. Zhou J. Europ. Ceram. Soc., 28 (2008) 2099–2107
  • 23.In Situ Reaction Synthesis, Electrical and Thermal, and Mechanical Properties of Nb4AlC3
    C. F.Hu, F. Z.Li, L. F.He, J Zhang, J. M.Wang, Y. W.Bao, J. Y.Wang, Y. C.Zhou J. Am. Ceram. Soc., 91 [7] 2258–2263 (2008)
  • 24.Synthesis, Microstructure, and Mechanical Properties of Al3BC3
    F. Z.Li, Y. C.Zhou, L. F.He, B Liu, J. Y.Wang J. Am. Ceram. Soc.,91 [7] 2343–2348 (2008)
  • 25.Kinetics and Mechanism of Hot Corrosion of γ-Y2Si2O7 in Thin-Film Na2SO4 Molten Salt
    Ziqi Sun, Meishuan Li, Yanchun Zhou J. Am. Ceram. Soc.,91 [7] 2236-2242 (2008)
  • 26.Preparation and Properties of Machinable Si2N2O/BN Composites
    Q. F. Tong, Y. C. Zhou, J Zhang, J. Y. Wang and M. S. Int. J. Appl. Ceram. Technol., 5 [3] 295–304 (2008)
  • 27.Atomic-scale microstructure and elastic properties of quaternary Zr–Al–Si–C ceramics
    Z.J. Lin, L.F. He, J.Y. Wang, M.S. Li, Y.W. Bao, Y.C. Zhou Acta Materialia 56 (2008) 2022–2031
  • 28.Ab initio modeling of the formation and migration of monovacancies in Ti2AlC
    T Liao, Jingyang Wang and Yanchun Zhou Scripta Materialia 59 (2008) 854–857
  • 29.Experimental and thermodynamic study of the hydrothermal oxidation behavior of Ti3SiC2 powders
    H.B. Zhang, X. Wang, K.G. Nickela, and Y.C. Zhou Scripta Materialia 59 (2008) 746–749
  • 30.MImproving the high-temperature oxidation resistance of Zr2Al3C4 by silicon pack cementation
    L.F. He, Y.W. Bao, M.S. Li, J.Y. Wang, and Y.C. Zhou J. Mater. Res., 23(8) (2008) 2275-2282
  • 31.Tailoring Texture of γ-Y2Si2O7 by Strong Magnetic Field Alignment and Two-Step Sintering
    Z. Q. Sun, X. W. Zhu, M. S. Li, Y. C. Zhou and Y. Sakka, J. Am. Ceram. Soc., 91 [8] 2521–2528 (2008)
  • 32.Thermal Properties and Thermal Shock Resistance of γ-Y2Si2O7
    Ziqi Sun, Yanchun Zhou, Jingyang Wang and Meishuan Li J. Am. Ceram. Soc., 91 [8] 2623–2629 (2008)
  • 33.Temperature Dependence of Elastic Properties for Amorphous SiO2 by Molecular Dynamics Simulation
    LIU Bin, WANG Jing-Yang, ZHOU Yan-Chun, LI Fang-Zhi Chin. Phys. Lett., 25(8)2008: 2747-2750
  • 34.Mechanical properties and damage tolerance of Y2SiO5
    Ziqi Sun, Jingyang Wang, Meishuan Li, Yanchun Zhou J. Europ. Ceram. Soc., 28 (2008) 2895–2901
  • 35.First-principles investigation of intrinsic defects and (N, O) impurity atom stimulated Al vacancy in Ti2AlC
    Ting Liao,Jingyang Wang and Yanchun Zhou, Appl. Phys. Lett., 93, 261911 2008