  • 1. Y. W. Bao, J. X. Chen, X. H. Wang and Y. C. Zhou

    Shear strength and shear failure of layered machinable Ti3AlC2 ceramics  J. Europ. Ceram. Soc., 24(5)855-860 (2004)

  • 2. J. X. Chen and Y. C. Zhou

    Strengthening of Ti3AlC2 by incorporation of Al2O3  Scripta Mater. 50(6)897-901(2004)

  • 3. Y. C. Zhou and W. L. Gu

    Chemical reaction and stability of Ti3SiC2 in Cu during high temperature processing of Cu/Ti3SiC2 composites

    Z. Metallkd., 95(1)50-56(2004)

  • 4. J. Y. Wang and Y. C. Zhou

    Polymorphism of Ti3SiC2 ceramic: first-principles investigations  Phys. Rev. B 69,144108 (2004)

  • 5. J. Y. Wang and Y. C. Zhou

    Ab initio elastic stiffness of nano-laminate (MxM2-x)AlC )(M=Ti, V, Nb and Cr) solid solution

    J. Phys.: Condens. Matter 16, 2819-2827 (2004)

  • 6. Y. C. Zhou, H. Y. Dong and X. H. Wang

    High temperature oxidation behaviour of polycrystalline Ti2SnC ceramic  Oxid. Metal. 61 (5/6)365-377(2004)

  • 7. Y. C. Zhou, B. Q. Chen, X.H. Wang and C.K. Yan

    Mechanical properties of Ti3SiC2 particulate reinforced copper matrix composites prepared by hot pressing of Cu-coated Ti3SiC2 and Cu powders

    Mater. Sci. and Tech.20(5) 661-665(2004)

  • 8. Y. C. Zhou, H. B. Zhang, M. Y. Liu. J. Y. Wang and Y. W. Bao

    Preparation of TiC free Ti3SiC2 by with improved oxidation resistance by substitution of Si with Al

    Mater. Res. Innovat. 8(2)97-102 (2004)

  • 9. H. B. Zhang, Y. C. Zhou, Y. W. Bao, M. S. Li

    Mechanism for the enhanced oxidation resistance of Ti3SiC2 by forming a Ti3Si0.9Al0.1C2 solid solution

    Acta Mater. 52(12)3631-3637 (2004)

  • 10. R. Z Huang, Y M Wang, J Y Wang and Y C Zhou

    First-principles investigations of stability and electronic structure of ZrV2Hx (x=0.5, 1, 2,3,4,6 and 7)

    Acta Mater 52(12) 3499-3506 (2004)

  • 11. M. Li, Y. Qian, Y. Li, Y. Zhou

    Beneficial effects of Ce implantation into preformed Cr2O3 scales on the subsequent oxidation of Ni-20Cr alloy

    Oxid. Metal 61(5-6) 529-544 (2004)

  • 12. J. Y. Wang and Y. C. Zhou

    Dependence of elastic stiffness on electronic band structure of nano-laminate M2AlC (M=Ti, V, Nb and Cr) ceramics

    Phy. Rev. B 69(21)21411(2004)

  • 13. X. M. Liu and Y. C. Zhou

    Seed-mediated synthesis of uniform ZnO nanorods in the presence of poly ethylene glycol

    J. Crys. Grow. 270(3-4) 527-534 (2004)

  • 14. Y. W. Bao and Y. C. Zhou

    Punch-shear tests and size effects for evaluating the shear strength of machinable ceramics

    Z Metalkd. 95(5)372-376(2004)

  • 15. Y. W. Bao and Y. C. Zhou

    Mechanical properties of Ti3SiC2 in bending at high temperature  Acta Metal. Sinica 17(4)465-470 (2004)

  • 16. X. H. Wang and Y. C. Zhou

    Hot corrosion of Na2SO4-coated Ti3AlC2 in air at 700-1000oC  J. Electrochem. Soc.,151(9)B505-511 (2004)

  • 17. X. L. Ma, Y. L. Zhu, X. H. Wang, Y. C. Zhou

    Microstructure characterization of the bulk Ti3AlC2 ceramics  Phil. Mag. 84(28)2969-2977(2004)

  • 18. Y. H. Quan, M. S. Li, L. Xin and Y. C. Zhou

    Investigation of growth stresses in NiO scale formed on Ni at 1000oC by a modified deflection method

    Mater. Res. Bull. 39(13)1985-1992(2004)